Thermal Conductivity Test ApparatusValue at mean temperature as per IS: 3346 – 1980. Testing of K value of Mineral wool insulation, Polypro ethane foam, expended Polystyrene, test is required to be done at a constant temperature of 0° to (-)10°C. Two slab guarded Hot Plate Method. Hot face Max. temperature (+99°C) Hot face Min. temperature (+60°C) Cold face max. temperature (+60°C) Cold face min. temperature (-10°C) Specimen size to be tested 300 m.m. X 300 m.m. Thickness 50 m.m. The above parameters will limit the testing range from 30°C to 99°C mean temperature. Water circulation system. Insulated Box with viewing window. The system also incorporated with accidental protection devices. thyrestorized firing heat control Designed as per IS: 3346 – 1980 Hot plate method. 2. Microprocessor based testing system consist of followings. 8 Channel scanner with all input flashing as per the pre programmed interval. Options:
- A computer with Powerlog software with necessary printer output will be there on the instruments.
- Thermal conductivity value to be calculated and as per the formula provided in our instruction manual.
- Hot plate system has got digital control for guard heater Temperature, needs only power supply and a few liters of water to operate.
- Stabilized voltage control system (Power Module) servo assisted To keep the voltage ±1 Volts.
Center Heater size:- 153 m.m. X 153 m.m. Specimen size to be tested – 300 m.m. X 300 m.m. Thickness: 50 m.m. Horizontal system. The ambient temperature of 27°C ±1C to be maintained by user.

|